Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sintering (2014)
Attributed to:
Material Systems for Extreme Environments
funded by
EPSRC
Abstract
No abstract provided
Bibliographic Information
Digital Object Identifier: http://dx.doi.org/10.2109/jcersj2.122.271
Publication URI: http://dx.doi.org/10.2109/jcersj2.122.271
Type: Journal Article/Review
Parent Publication: Journal of the Ceramic Society of Japan
Issue: 1424